SP-3

SPECIAL FILM FOR POWER PRESTRECH

 

Physical and mechanical properties*

STANDARD

M.D

U.M.↓

T.D →

TOLERANCE

Yield tensile stress

ASTM D882-88

 

N/mm2

 

7.7

 

8.2

 

5%

Tensile stress at break

ASTM D882-88

 

N/mm2

 

40

 

27

 

5%

Elongation at break

ASTM D882-88

 

%

 

590

 

829

 

5%

Puncture elongation

METHOD DOW

mm

 

119

 

119

 

10%

Tear resistance

ASTM D1922-67

mn

 

220

 

324

 

10%

Impact resistance

ASTM  1709-75D

g

 

220

 

220

 

10%

Guaranteed prestretch

METHOD SAPIR PLASTIC

%

 

190

 

 


* All above data refer to the following conditions:

- Thickness: 23 micron.

- Temperature: 20 c

The information appearing in this technical specification reference is accurate according to quality tests that were done by us in the plant. Since various factors may influence that technical data, the above specifications don’t carry any legal obligation or liability. The customer/user must check the data in the above specification reference in order to achieve the best results.